I believe some washing difficulties relate to how dry the masks get. They have to be rehydrated before washing off, so if too dry, this can take a longer time. Most of them have constituents which help keep some moisture in them, but time and temperature will increase dryness. Regards, Peter -------------------------------------------------------- Peter Swanson [log in to unmask] INTERTRONICS http://www.intertronics.co.uk Tel: +44 1865 842842 Oxfordshire, England INTERTRONICS is dedicated to providing quality material, consumable and equipment solutions to the high technology, high performance assembly industries, incorporating outstanding levels of technical support and customer service. Read our news! http://www.intertronics.co.uk/blog/blog.htm -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: 23 May 2008 21:10 To: [log in to unmask] Subject: Re: [TN] Water soluble masking Hi Ioan! We use Techspray (the light blue stuff) here, and don't have any problems. We even mask boards on Friday, leave them set over the weekend, then wave them Monday, and they clean fine for us. We have a Technical Devices In-line cleaner running deionized water at about 150 F., at a belt speed of around 4 fpm, and haven't had any problems. There's even been a few occasions that boards have been accidently left in a 180 F. oven (meant to speed the cure of the mask) over the weekend and they have still cleaned fine after wave. Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea Sent: Friday, May 23, 2008 2:53 PM To: [log in to unmask] Subject: [TN] Water soluble masking Dear Technos, I am testing WS solder masking substances and what I see is that they wash perfectly if relatively fresh (barely cured or after a couple of hours on the board) and they wash very poorly if passed in the in-line machine 24 or 48 hours after the application. Is this natural? What is your experience? Chemtronics have a note on the bottle requesting washing within 48 hours, nothing marked on the Techspray bottle, but both are very difficult to remove after 24 hours. Thanks, Ioan --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------