Here's a link to the NASA web page about zinc whiskers:
http://nepp.nasa.gov/WHISKER/reference/tech_papers/Brusse2003-Zinc-Whisk
er-Awareness.pdf
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dennis Fritz
Sent: Friday, April 24, 2009 11:54 AM
To: [log in to unmask]
Subject: Re: [TN] Zinc Plating and whiskers
Roger,
NASA reports they are being called in as much these days on zinc
whiskers issues, as on tin whiskers.? The structural steel for raised
computer room floors seems to be the most common culprit.? Why is that a
problem?? Zinc whiskers get broken off into the recirculated air flow
used for cooling the big servers.? They re-deposit conductive filaments
onto operating circuit boards, and poof !!? - you've blown some bits of
information due to the short.? Maybe you can't even figure out where the
transient voltage spike came from .? Dig further into the NASA web
site.?
Not nearly as much work has been done on causes of whiskers?with zinc
over steel, compared to tin over copper.? I don't know which zinc
electrolyte platings are the worst.
Denny Fritz
-----Original Message-----
From: EIMCNews <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, 24 Apr 2009 11:44 am
Subject: Re: [TN] Plating on screws
Dave,
I've been around plating a lot, especially zinc and I never heard of
zinc whisker formation. Are you sure you don't mean tin whisker
formation?
If you really do mean zinc please direct me to some information about
it.
It's never too late in life to learn something new.
Sincerely,
Roger Mouton
EIMC - Advanced Plating Technologies
949 481-5194
www.smartcatshield.com
[log in to unmask]
Notice of Confidentiality
The information contained in and transmitted with this email may be
confidential and is intended only for the individual or entity named
above.
If you are not the intended recipient, you are hereby notified that
inadvertent disclosure of this information to you does not constitute a
waiver of confidentiality privilege and that any review, disclosure,
copying, or use of the contents of the email by you is prohibited.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|