Cost too.
The ballpark cost of a machine to add balls is ~$300K...
Joyce Koo wrote:
> Mostly due to performance. Rf device for example.
> --------------------------
> Sent using BlackBerry
>
>
> ----- Original Message -----
> From: TechNet <[log in to unmask]>
> To: [log in to unmask] <[log in to unmask]>
> Sent: Thu Apr 16 10:47:07 2009
> Subject: Re: [TN] LGAs in a military environment?
>
> Why aren't these parts BGA's anyway? Is it just the extra inductance? Or is it because putting on solder balls costs money?
>
> I'd send them out and get real balls put on them. You may need to limit the solder joint height due to potential parasitic issues, but I'm guessing that 0.15mm (6mils) joint height would not kill the performance and would substantially improve all aspects of reliability. (Underfill may be required to achieve thermal rqmts)
>
> Wayne Thayer
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Temkin, Gregg
> Sent: Thursday, April 16, 2009 10:29 AM
> To: [log in to unmask]
> Subject: Re: [TN] LGAs in a military environment?
>
> Our failures were by analysis only. We did not go into production with these parts. We were evaluating the fatigue reliability of the solder joints. We tend to be very conservative in our design approach, but we have to be, since we're building hardware that controls the primary power systems in aircraft. We also have generally steered away from QFN parts for the same reasons.
>
> At my former employer we designed a product with QFN microcontrollers. We had a very high percentage of failed solder joints after ESS. That company's quality systems and ethics were pretty sketchy, so the parts would go through a rework cycle and if they passed ESS after that, the product was shipped. No cause was assigned, everything was considered an "isolated failure". That product hasn't yet made it to the field (tied to a long development military helicopter program) so the field failure rate is yet to be seen, but it's obviously not going to be good. Fortunately it's not too critical a piece of hardware.
>
> Gregg
>
>
> -----Original Message-----
> From: kwood716 [mailto:[log in to unmask]]
> Sent: Thursday, April 16, 2009 6:40 AM
> To: 'TechNet E-Mail Forum'; Temkin, Gregg
> Subject: RE: [TN] LGAs in a military environment?
>
> Gregg,
> What were the failures? I'm interested because I see LGA usage picking up steam here.
> Ken
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Temkin, Gregg
> Sent: Thursday, April 16, 2009 9:22 AM
> To: [log in to unmask]
> Subject: Re: [TN] LGAs in a military environment?
>
> We just designed out similar LGAs made by Linear when a reliability analysis showed VERY EARLY failures probabilities for our typical operation cycle over a 20 year life.
>
> You can certainly get them soldered and have them pass a screen but that may not be the whole picture. Depends on your operating environment/life requirements. Suggest having someone who is good at analysis run the numbers.
>
> Gregg
>
> -----Original Message-----
> From: Graham Collins [mailto:[log in to unmask]]
> Sent: Thursday, April 16, 2009 3:32 AM
> To: [log in to unmask]
> Subject: [TN] LGAs in a military environment?
>
> Hello Technet!
> One of our designers is advocating using a LGA component in a military product. Anyone out there doing it? I'm wondering (worried) about the reliability since it has a very low standoff. And cleaning issues?
>
> An example of the parts I'm referring to:
> http://www.linear.com/designtools/packaging/lga/05081807_a_lga66.pdf
> A Linear Technologies p/n LTM4604
>
> regards,
>
> Graham Collins
> Halifax Production Engineering
> (902) 873-2000 ext. 6215
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
> Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
--
Eric Christison Msc
Mechanical Engineer
Consumer & Micro group
Imaging Division
STMicroelectronics (R&D) Ltd
33 Pinkhill
Edinburgh EH12 7BF
United Kingdom
Tel: +44 (0)131 336 6165
Fax: + 44 (0)131 336 6001
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|