TECHNET Archives

March 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 12 Mar 2001 20:59:18 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Fish <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
David Fish <[log in to unmask]>
Parts/Attachments:
text/plain (78 lines)
We've seen this caused by:
*  Static charge of components that are small relative to their pocket [may
be winter time - low humidity - related, also.].  Seek relief with an
ionizer bar over feeder bank.
*  Adhesive [from cover tape??] on component.  Some of these were so
gummed-up that when able to be picked, they would not give-up the nozzle
even when the nozzle was removed from the machine.  Seek relief by mugging
the supplier.
*  Adhesive from cover tape attaches component to cover tape.  Seek relief
by ...

Dave Fish

----- Original Message -----
From: bbarr <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, March 09, 2001 1:46 PM
Subject: [TN] Part Sticking to Top Tape?


> I have two different part numbers of a surface mount resistor array that
> feeds out of a 12mm tape. This is the problem with both: The back end of
the
> part wants to ride up with the tape at the tape peel back point. They look
> like little soldiers laying on top of the tape. I say the back edge is
> riding up because the parts are marking side up and I don't see the part
> actually flipping. The part is .200 x .120 so we are not talking a real
> small part here. Is this a static problem? Even when the part is in the
> pocket just before the tape peel back point it seems like it is attracted
to
> the tape because the front edge of the part is raised up against the tape.
> Anyone else experience this? To get the boards built I fabricated a little
> piece of metal and taped it to the top of the feeder to keep the part in
the
> pocket. Not too elegant and I would really like to know what is going on
> here. I even tried blowing air from an ionizer fan on the reel to see if I
> could neutralize a charge, but that did not help.
>
> Thanks.
>
>
> Bob
>
>
> Robert Barr
> Manufacturing Engineering
> Formation, Inc.
> Voice: 856-234-5020 x3035
> Fax: 856-234-6679
> email: [log in to unmask]
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2