TECHNET Archives

February 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 10 Feb 2012 10:01:01 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Message-ID:
Subject:
From:
Thomas E Kemp <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (45 lines)
I'm not at liberty to say how we do it, but we do it every day. Yes, there 
are some real issues if not done correctly.
Tom



John Burke <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
02/10/2012 09:48 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
<[log in to unmask]>


To
<[log in to unmask]>
cc

Subject
[TN] Silver immersion with gold fingers






Having some issues with silver immersion on a board with gold pated 
fingers - anyone having success with this?

Issue apparently is in masking off the gold during the silver process.

John

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2