TECHNET Archives

September 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 6 Sep 2006 23:05:14 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hfjord <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
8bit
Content-Type:
text/plain; format=flowed; charset="UTF-8"; reply-type=original
From:
Parts/Attachments:
text/plain (60 lines)
Bad pull force?
Inge



----- Original Message -----
From: "Werner Engelmaier" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, September 05, 2006 3:50 PM
Subject: Re: [TN] Pad pull force


In a message dated 9/5/06 0:45:08, [log in to unmask] writes:
> Is there a standard that defines a minimum pull force requirement after
> the
> component has been soldered.
> A: No, there is no such standard. A properly wetted solder joint is
> stronger
than the attachment of the soldering pads to the PCB/component resin matrix.

> The issue is, to get a better joint we had introduced extra solder to the
> component (confirms to IPC-610D).
> A: Why do you think that more solder will give you a "better joint"? What
does better mean?

> Do we have a minimum pull force value which can be adopted so
> that we can give assurance to customer that there will be no issue with
> joints.
> A: Solder joint issues come from either low quality—meaning inadequate
metalurgical bond due to insufficient wetting; or from creep-fatigue which
is not
very dependent on solder joint volume. So, you are reallly asking the wrong
question.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2