John,
In todays world, if a PCB is properly cleaned after etch, deposition and
prior to mask, then acid traps should not be a concern.
We do a lot of weird angle stuff in the RF world and I have never seen a
failure due to acid trap type issues.
Bottom line is if your fabricator has good process then it should not be
an issue, but to keep risk to a minimum good design practice should be
followed when possible.
Hope it helps,
FNK
Frank N Kimmey CID+
Principal PCB Designer
PCB Programs
Powerwave Technologies Inc
Office 916-941-3159
Fax 916-941-3195
Mobile 916-670-0645
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Foster
Sent: Tuesday, November 21, 2006 8:53 AM
To: [log in to unmask]
Subject: [TN] Acid Traps
I would like to ask the board fabricators if acid traps are a real
issue.
I normally try to avoid any feature that creates a structure that is
less
then 90 degrees.
However I am helping out another group by reviewing their boards and
there
are literally
hundreds of acid traps on the board. This board is class 3 and has to be
high reliability.
I have always been taught that they can be a real problem. But have
never
quite understood
why.
Any input on this will really be appreciated.
Thanks
John Foster
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|