TECHNET Archives

May 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 8 May 2001 08:25:59 -0500
Content-Type:
multipart/mixed
Parts/Attachments:
text/plain (471 bytes) , TEXT.htm (831 bytes)
It is possible to have insufficient adhesive and the solder tension from the wave washed the parts away.  Do the glue dots have a mounded or flat appearance?  How are you dispensing the adhesive?  What component packages are you seeing this with (1 type, various types, etc).  What type of wave machine do you use?  Is it a flat wave or angled?  Do you have a chip wave also operating at this time?  What is the speed of the conveyor?  What is the wave depth?

Kathy 



<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN"> <HTML><HEAD> <META content="text/html; charset=iso-8859-1" http-equiv=Content-Type> <META content="MSHTML 5.00.2614.3500" name=GENERATOR></HEAD> <BODY style="FONT: 10pt Haettenschweiler; MARGIN-LEFT: 2px; MARGIN-TOP: 2px"> <DIV>It is possible to have insufficient adhesive and the solder tension from the wave washed the parts away.&nbsp; Do the glue dots have a mounded or flat appearance?&nbsp; How are you dispensing the adhesive?&nbsp; What component packages are you seeing this with (1 type, various types, etc).&nbsp; What type of wave machine do you use?&nbsp; Is it a flat wave or angled?&nbsp; Do you have a chip wave also operating at this time?&nbsp; What is the speed of the conveyor?&nbsp; What is the wave depth?</DIV> <DIV>&nbsp;</DIV> <DIV>Kathy </DIV></BODY></HTML>