We've applied conformal coating for that application. You need some tough
stuff.
Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com
On Thu, Jun 5, 2014 at 8:12 AM, Graham Collins <[log in to unmask]>
wrote:
> My understanding is that the device can be expected to see 170 C.
>
> regards,
>
> Graham Collins
> Senior Process Engineer
> Sunsel Systems
> (902) 444-7867 ext 211
>
> On 6/4/2014 4:51 PM, Stadem, Richard D. wrote:
>
>> What temperatures will the device see (both external and internal) in the
>> field?
>> There are companies that make equipment for monitoring lava temperatures.
>> If they can do that, then the inside of an oil well should be pretty ho
>> hum.....
>>
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
>> Sent: Wednesday, June 04, 2014 2:19 PM
>> To: [log in to unmask]
>> Subject: [TN] high temp environment
>>
>> Hello Technet!
>> We are discussing an opportunity with a customer who is looking at
>> placing an instrument down-hole in an oil well, hence a high temp
>> environment. Are there any good resources around to help me with this one?
>> Obviously I need high temp solder (Sn96Ag4?), the components will have to
>> be carefully picked, and we will need PWBs that will be OK at high temp
>> (polyimide?).
>>
>> I've got some homework to do! :-)
>>
>> --
>> regards,
>>
>> Graham Collins
>> Senior Process Engineer
>> Sunsel Systems
>> (902) 444-7867 ext 211
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|