Back in the day, we would have approached as much as we could with hybrid
technology.
Eutectic die attach on ceramic [High temp co-fired ceramic, alumina
substrate within metal package, or Low Temp Co-fired ceramic], etc. Way
back, there was even eutectic attach for passives - if properly
metallized...
Being in a hermetic package, no conformal coatings...
Being a potentially highly corrosive environment the package is truly put to
the test. Drawing upon implantable medical technologies [also a corrosive
environment, believe it or not], there are multiple packaging options
available including stainless & titanium.
Just a different persective...
Steve Creswick
Sr Associate - Balanced Enterprise Solutions
http://www.linkedin.com/in/stevencreswick
616 834 1883
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|