We use Minico M-5010-CR carbon ink from:
 W.R. Grace & Co		
5210 Philip Lee Dr.
Atlanta, GA 30336
(404)699-3355
(404)699-3332 FAX
Minico Polymer Thick Film

We screen print it with an Autooroll and bake it twice.  The stuff is available in different 
resistance formulations  from 1 ohm per square to 100 ohms per square.  It is pretty easy to screen 
as long as you have good ventilation in the screening area (strong solvent odor).

DuPont has a similar product called E81072 Conductive Carbon Coating.  I have the data sheets and a sample.  It smells less than the Minico ink so the operators prefer it.  Unfortunately the data sheet says it is only available in 24-27 ohms per square.  They may have other flavors.  You can call John Crosby at
DuPont
Richmond, VA
(804)745-2706
(800)217-6261 pager  
[log in to unmask]
Good luck trying to reach him.  They spread him real thin.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2