Hi Wee Mei,
To echo what others have already said.
Your colleague can also check the manufacturer's coating thickness
recommendation for a specific product. (I'm sure that's where IPC-A-610 got
the numbers.)
I strongly recommend staying within the acceptable range. My personal
preference is to target slightly higher than the middle of the spec., if the
range is broad enough. I've run into problems, on the processing side, when
someone specified well above the max. and we had hideous solvent retention.
Folks using conformal coating as a potting compound are not my friends.
Hans
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Electronics Engineer
Warner Robins - Air Logistics Center (WR-ALC/LUGE)
226 Cochran Street
Robins AFB GA 31098-1622
mailto:[log in to unmask]
Com: (478) 926 - 5224
Fax: (478) 926 - 4911
DSN Prefix: 468
-----Original Message-----
From: fullname [mailto:[log in to unmask]]
Sent: Thursday, May 30, 2002 10:27 PM
To: [log in to unmask]
Subject: [TN] Coating thickness
IPC-A-610C section 9.1.3 mentioned the following coating thickness :
Type AR Acrylic resin 0.03 - 0.13mm
Type ER Epoxy resin 0.03 - 0.13mm
Type UR Urethane resin 0.03 - 0.13mm
Type SR Silicon resin 0.05 - 0.21mm
Type XY Paraxlyene resin 0.01 - 0.05mm
Questions asked on behalf of my colleague are :
1. How does one arrive at the coating thickness for each types of
coating material?
2. What is the impact to my board or components if my coating thickness
exceed or below the range stated above?
Regards - Wee Mei
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|