Having formulated a number of UV curable solder masks in previous years, I
do know that the IPC used to have a specs that required exposure to
solvents, including methylene chloride. With UV's, more cure equals a
higher crosslink density...and hence....better resistance to solvents (and
flux absorption). There is instrumentation to help characterize cure, but
it is not straight forward for the average user. Thermal cure chemistries
generally give (gave) better performance than UV's since many UV's use
smaller chain epoxy acrylate monomers (diluents) that just don't offer as
much bond strength as polymers with BPA resins.
-----Original Message-----
From: Leigh Jansen [mailto:[log in to unmask]]
Sent: Monday, July 14, 2003 12:55 PM
To: [log in to unmask]
Subject: [TN] SOLDER RESIST COMPATIBILITY
Importance: High
Dear All,
can anyone kindly quote me any specific standards which relate to either the
degree of cure of solder resists (I know of a BS standard which uses 3
different solvent rubs but can't remember the number..) or, which relate to
the compatibility of the resist with coating strippers ??
As I am not an expert in solder resists but generally I thought they were
epoxy based and if cured properly, pretty resistant to even the likes of
Methylene Chloride ?
Many thanks in advance,
Leigh Jansen
Technical Support Manager
Concoat Limited - Engineering Electronics Reliability
Web: www.concoat.co.uk AND www.concoatsystems.com
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|