Dan
Theoretlically, you can use your 5 zone oven. FIgure on, ballpark, about 20
- 25% less through-put for the lead-free profile with the higher thermal
excursion, depending upon whether you prefer to use a straight-ramp or "classic"
ramp-soak-spike profile.
The best way to tell is to take a typical lead-free profile from a lead-free
supplier spec and attempt to profile your most complicated PCBAs to that
profile. If you can do it with your existing 5 zone, albeit at a slower conveyor
speed, you're home free. If not, it might be time to go shopping.
You better believe that the oven and wave-solder manufacturers are seeing a
"Y2K" effect with respect to 7-1-06.
Phil Zarrow
ITM Consulting
Durham, NH USA
603 868-1754
www.ITMconsulting.org
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|