I have seen this occur many times. In fact, it was a persistent problem where I was working until we resolved it. Ask Engelmaier about worms, types I II or III.
Best regards
Lee
J. L. Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: Franklin D Asbell<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Wednesday, April 20, 2005 5:47 PM
Subject: Re: [TN] Peeling Copper traces
If there were resist residue I would think it would probably not plate up at
all...at least this is what I observe...
Franklin
----- Original Message -----
From: "Lee parker" <[log in to unmask]<mailto:[log in to unmask]>>
To: <[log in to unmask]<mailto:[log in to unmask]>>
Sent: Wednesday, April 20, 2005 4:17 PM
Subject: Re: [TN] Peeling Copper traces
Rich
If the boards are pattern plated, check for photo resist residue between the
copper layers.
Best regards
Lee
J. L Parker Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: Rich Olsen<mailto:[log in to unmask]<mailto:[log in to unmask]>>
To: [log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]>>
Sent: Wednesday, April 20, 2005 4:50 PM
Subject: [TN] Peeling Copper traces
Hello,
What are some likely causes of peeling copper traces?
It is plated copper pulling away from the foil copper?
thanks,
Rich
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to
[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]>> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]>>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]>>: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives<http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>>
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>>
for additional information, or contact Keach Sasamori at
[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]>> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|