TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Date:
Wed, 20 Apr 2005 19:49:14 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Lee parker <[log in to unmask]>
Parts/Attachments:
text/plain (109 lines)
Franklin

I have seen this occur many times. In fact, it was a persistent problem where I was working  until we resolved it. Ask Engelmaier about worms, types I II or III.

Best regards

Lee

J. L. Parker, Ph.D.
JLP Consultants LLC
804 779 3389
  ----- Original Message ----- 
  From: Franklin D Asbell<mailto:[log in to unmask]> 
  To: [log in to unmask]<mailto:[log in to unmask]> 
  Sent: Wednesday, April 20, 2005 5:47 PM
  Subject: Re: [TN] Peeling Copper traces


  If there were resist residue I would think it would probably not plate up at
  all...at least this is what I observe...

  Franklin


  ----- Original Message -----
  From: "Lee parker" <[log in to unmask]<mailto:[log in to unmask]>>
  To: <[log in to unmask]<mailto:[log in to unmask]>>
  Sent: Wednesday, April 20, 2005 4:17 PM
  Subject: Re: [TN] Peeling Copper traces


  Rich

  If the boards are pattern plated, check for photo resist residue between the
  copper layers.

  Best regards

  Lee

  J. L Parker Ph.D.
  JLP Consultants LLC
  804 779 3389
    ----- Original Message -----
    From: Rich Olsen<mailto:[log in to unmask]<mailto:[log in to unmask]>>
    To: [log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]>>
    Sent: Wednesday, April 20, 2005 4:50 PM
    Subject: [TN] Peeling Copper traces


    Hello,

            What are some likely causes of peeling copper traces?
            It is plated copper pulling away from the foil copper?

    thanks,
    Rich

    ---------------------------------------------------
    Technet Mail List provided as a service by IPC using LISTSERV 1.8e
    To unsubscribe, send a message to
  [log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]>> with following text in
    the BODY (NOT the subject field): SIGNOFF Technet
    To temporarily halt or (re-start) delivery of Technet send e-mail to
  [log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]>>: SET Technet NOMAIL or (MAIL)
    To receive ONE mailing per day of all the posts: send e-mail to
  [log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]>>: SET Technet Digest
    Search the archives of previous posts at:
  http://listserv.ipc.org/archives<http://listserv.ipc.org/archives<http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>>
    Please visit IPC web site
  http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>>
  for additional information, or contact Keach Sasamori at
  [log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]<mailto:[log in to unmask]>> or 847-615-7100 ext.2815
    -----------------------------------------------------

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
  for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or
  847-615-7100 ext.2815
  -----------------------------------------------------

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
  -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2