Ken,

It's OK and even recommended per IPC 7721. Technique is covered in 2
procedures that both call for using flat copper ribbon material. You can see
similar procedures on our web site at:
http://www.circuittechctr.com/guides/4-2-1.htm and
http://www.circuittechctr.com/guides/4-2-1.htm.

We always use this techniques vs. jumper wires for short breaks in
conductors.

Jeff Ferry
CEO
Circuit Technology Center
www.circuittechctr.com
[log in to unmask]

Chairman
IPC Repairability Committee

-----Original Message-----
From: Ken Patel [mailto:[log in to unmask]]
Sent: Tuesday, February 06, 2001 8:26 PM
To: [log in to unmask]
Subject: Is it acceptable trace rework?


Guys,
Initially, we had a trace cut and then we decided that we don't need that
trace cut. So on few boards, our CM told us that they can fix the trace by
putting a small trace across the cut out and soldered the ends. Also, put
some kind of solder masking on top of that soldered traces. Is it
acceptable? Any comments from experience folks. Or should I go for real
jumper wire.

re,
ken patel

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2