The dilemma for Dewey and IPC-4101 is that this is raw materials specs.
You might say it govern laminate mfg and incoming inspection.
BUT, it doesn't cover the APPLICATION, USE, COSTS and RELIABILITY, and it
can't.
Electronics is such a BROAD FIELD, that the simple slash sheets are going
to be applied from:
2-sided to 40-layer,
from 18 months life to 20 years,
from 0.020" to 0.300" thickness,
from tin-lead soldering to CuSn soldering,
from no-rework to 3X rework cycles.
All of these conditions require something different from the raw laminates
and prepregs.
Dewey in the committee meeting talked about a "Finish Multilayer Standard
for Materials" that was needed, because the IPC-4101 A/B Slash Sheets
can't possibly be adjusted to cover all the cases above.
Happy Holden
Asian Pacific Materials
Werner Engelmaier <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/26/2006 09:44 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
Re: [TN] Rohs Weeeeeee board material
Hi Doug,
Of course I do not suggest Tg 178 instead of 175; but the slash sheets
give
ranges on the same sheet thast include Tg's with 50 degree
differences--they
should perhaps be no ore than about 20.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|