TECHNET Archives

August 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Chares Dennehy <[log in to unmask]>
Date:
Tue, 5 Aug 2008 15:20:47 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Steve Gregory <[log in to unmask]>
Parts/Attachments:
text/plain (48 lines)
Hi Charley!

I was just getting ready to toss some Kester PB93.5/Sn5/AG1.5 RMA
44-flux in with our dross buckets for recycling...we don't do HMP stuff
anymore. The rolls are still in the vacuum sealed packaging, but the
date of manufacture is 07/15/03. I think it still should be okay
though...

Steve 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chares Dennehy
Sent: Tuesday, August 05, 2008 2:16 PM
To: [log in to unmask]
Subject: [TN] High temperature solder

Do any of you Technetters have a source from which to order a roll or
two (as opposed to ten roll minimum) of high temperature, wire core
solder.  I'm looking for something like Pb90 / Sn10 or some such solder
that has a reflow temp (low end of plastic range) above 250C.  

Charley

 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2