Hi Charley! I was just getting ready to toss some Kester PB93.5/Sn5/AG1.5 RMA 44-flux in with our dross buckets for recycling...we don't do HMP stuff anymore. The rolls are still in the vacuum sealed packaging, but the date of manufacture is 07/15/03. I think it still should be okay though... Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Chares Dennehy Sent: Tuesday, August 05, 2008 2:16 PM To: [log in to unmask] Subject: [TN] High temperature solder Do any of you Technetters have a source from which to order a roll or two (as opposed to ten roll minimum) of high temperature, wire core solder. I'm looking for something like Pb90 / Sn10 or some such solder that has a reflow temp (low end of plastic range) above 250C. Charley --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------