Ed,
If the minor chemical constituents in the CFC based cleaners didn't foul you
up, then n-propyl bromide won't.
regards,
Bev Christian
Nortel
PS Not all n-propyl bromides are the same purity, but this statement is not
meant as a reflection on the supplier you mentioned.
> ----------
> From: Edward Boucher[SMTP:[log in to unmask]]
> Sent: Wednesday, July 15, 1998 4:05 PM
> To: [log in to unmask]
> Subject: [TN] N-Proply-Bromide (Ensolv) compatability with Uralane
> 5753 and 5750
>
> Greetings Technet,
>
> In 1992 we had a aerospace application where we required the use of
> Uralane 5753 (conformal coating) and Uralane 5750 (potting). The Uralane
> Mfg. is Ciba Specialty Chemicals. At that time
> portions of our cleaning process called for the use of Genesolve and Freon
> (TMS). Our concern is whether or not there are cure inhibitions or
> adhesion problems when using N-Proply-Bromide(Ensolv) with Uralane 5753
> and
> 5750 in standard electronic manufacturing processes.
>
> Please advise with any pertinent information or direction.
>
> Thank you Ed Boucher
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|