TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Bev Christian <[log in to unmask]>
Date:
Wed, 15 Jul 1998 23:11:33 -0400
MIME-Version:
1.0
X-To:
Edward Boucher <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (60 lines)
Ed,
If the minor chemical constituents in the CFC based cleaners didn't foul you
up, then n-propyl bromide won't.

regards,
Bev Christian
Nortel

PS Not all n-propyl bromides are the same purity, but this statement is not
meant as a reflection on the supplier you mentioned.

> ----------
> From:         Edward Boucher[SMTP:[log in to unmask]]
> Sent:         Wednesday, July 15, 1998 4:05 PM
> To:   [log in to unmask]
> Subject:      [TN] N-Proply-Bromide (Ensolv) compatability with Uralane
> 5753 and 5750
>
> Greetings Technet,
>
> In 1992 we had a aerospace application where we  required the use of
> Uralane 5753 (conformal coating) and Uralane 5750 (potting). The Uralane
> Mfg. is Ciba Specialty Chemicals.  At that time
> portions of our cleaning process called for the use of Genesolve and Freon
> (TMS). Our concern is whether or not  there are cure inhibitions or
> adhesion problems when using N-Proply-Bromide(Ensolv) with Uralane 5753
> and
> 5750 in standard electronic manufacturing processes.
>
> Please advise with any pertinent information or direction.
>
> Thank you Ed Boucher
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2