Kerry,
Pure tin balls?! I have not heard of that before. Pure tin melts considerably higher than SAC alloys. Hmm, 206C you say, 14 layer board? It is quite possible that your temperature/time is not enough to get a significant amount of diffusional mixing of the solder paste and the balls. But then you mention intermittents at the corners as well as the center.
Two other possibilities are warping of the part (but would expect that to give you intermittents in one or the other area, not both) or there is a severe problem with the construction of the component itself and there is internal damage to the component.
You don't say, but I presume the board itself solders well and there are no other soldering problems on the board that would lead you to suspect the solder paste?
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Kerry McMullen
Sent: May 23, 2005 1:10 PM
To: [log in to unmask]
Subject: [TN] BGA Intermittents
Hi Technetters,
I have a 1089 BGA with Sn balls.
Paste is 63/37 SnPb
Board is 14 layer, .098 thick Immersion Ag.
Ran thermocouples. Inner balls are seeing 206 degrees C.
What could be causing intermittents at the center and corners of the BGA?
Thanks,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Kerry
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|