TECHNET Archives

February 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w0F4w-0007zZC; Thu, 27 Feb 97 17:17 CST
Old-Return-Path:
Date:
Thu, 27 Feb 97 16:25:36 MDT
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
From [log in to unmask] Fri Feb 28 08:
56:49 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"OZeE23.0.QME.DOX5p"@ipc>
Subject:
From:
X-Loop:
X-Mailing-List:
<[log in to unmask]> archive/latest/10740
Message-Id:
Parts/Attachments:
text/plain (45 lines)
  For 90Pb10Sn, E is about 23 GPa at 0 degree C and 18 at 100 C. I guess that 
  of 95Pb5Sn is close. Look SRC/CINDAS Microelectronics Packaging Materials 
  Database, 4/95 for details where the properties of many alloys are listed.
  
  Yuan Li
  Exabyte


______________________________ Reply Separator _________________________________
Subject: Asmbly - Properties Data
Author:  [log in to unmask] at UNIXMAIL
Date:    2/22/97 6:04 AM


     Hi Technet - I am on a quest to find the Young's Modulus for two 
     alloys: 95Pb/5Sn and 90Pb/10Sn. Does anyone know what the values are 
     or a possible source? 
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2