TECHNET Archives

March 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Cheryl Tulkoff <[log in to unmask]>
Date:
Mon, 29 Mar 2004 15:12:39 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Cheryl Tulkoff <[log in to unmask]>
Parts/Attachments:
text/plain (32 lines)
Does anyone have any recommendations for batch cleaners?

I need to set up a small specialty cleaning process for a precison analog
card. I have to remove incoming parts contamination (chlorides, bromides,
sulfates) that our DI water wash process alone cannot remove. These
contaminants are causing leakage resistance failures in a critical part of
the circuit.

Out of three different parts vendors we tested using ion chromatography,
only 1 had a decent level of cleanliness and just barely met requirements.
The lab we used was able to remove the bulk of the parts contamination
with a saponified DI wash.

The part is a $.01 SOT-23 so our vendors are not very motivated to clean
up their act (pun intended). Our current Electovert Aquastorm 100 inline
cleaners cannot handle any chemistry so we're going to try and set up a
saponified cleaning process.

Any suggestions?

Thanks, Cheryl

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2