Does anyone have any recommendations for batch cleaners? I need to set up a small specialty cleaning process for a precison analog card. I have to remove incoming parts contamination (chlorides, bromides, sulfates) that our DI water wash process alone cannot remove. These contaminants are causing leakage resistance failures in a critical part of the circuit. Out of three different parts vendors we tested using ion chromatography, only 1 had a decent level of cleanliness and just barely met requirements. The lab we used was able to remove the bulk of the parts contamination with a saponified DI wash. The part is a $.01 SOT-23 so our vendors are not very motivated to clean up their act (pun intended). Our current Electovert Aquastorm 100 inline cleaners cannot handle any chemistry so we're going to try and set up a saponified cleaning process. Any suggestions? Thanks, Cheryl --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------