Hello Folks,
Could anyone help me explain how does silver migration occurs? We have had some problems like exposed silver glue meaning not covered totally by silicon encapsulant. Will this scenario lead to silver migration?
Allan J. Bareno
Process Engineer
Process Engineering Group Tel Nos. (632)8445139 ext.288
RF Personal Communications &Consumers (6349)5430001 to 25 ext 288
Philips Semiconductors Philippines Inc. Fax Nos. ( 6349) 5439368
Philips Avenue, Light Industry and Science Park 1 email: [log in to unmask]
Bo.Diezmo Cabuyao Laguna Philippines 4025
The information contained in this message is confidential and may be legally privileged. The message is intended solely for the addressee(s). If you are not the intended recipient, you are hereby notified that any use, dissemination, or reproduction is
strictly prohibited and may be unlawful. If you are not the intended recipient, please contact the sender by return e-mail and destroy all copies of the original message.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|