TECHNET Archives

July 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Buscomb, Scott" <[log in to unmask]>
Date:
Tue, 10 Jul 2001 08:59:21 -0400
MIME-version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Hiteshew, Michael" <[log in to unmask]>
Content-type:
text/plain
Subject:
From:
"Hiteshew, Michael" <[log in to unmask]>
Content-transfer-encoding:
7BIT
Parts/Attachments:
text/plain (75 lines)
Scott,
        The last time I looked the positional accuracy of a laser
photoplotter was about 1/4 mil (.00025"). Whatever feature to feature
tolerance you're concerned about will NOT be a function of imaging. What it
will be a function of is copper weight and etching/plating process control.
        Copper weight is a factor because as the copper gets thicker it gets
more difficult to etch it extremely accurately. After etching, traces have a
trapezoidal shape. The thicker the copper, the more the difference in width
between the top of the trapezoid and the bottom.
        The etching/plating process will vary from chemical batch to
chemical batch (as will the actual thickness of copper on the FR4).
        As a rule of thumb, assume your feature widths and spaces will vary
by approximately the thickness of the copper they're etched in. That is, an
8 mil trace may vary between 6.5 - 9.5 mils, and an 8 mil space may vary by
the same amount if etched in 1 oz/sqft (.0014" thick) copper. Most producers
typically do much better, but don't bet the farm on it. Greater accuracy can
be achieved in thinner copper weights or by paying more per piece.
        On the other hand, I may be misinterpreting the question. If your
concern is with mechanical design tolerances, that's a different issue. The
positional tolerance of components after they're mounted on the board will
be related to pad shape and size, as well as the positional tolerance of the
component leads. The larger the pad area the more the component can "drift",
but the easier they are to assemble (and vice-versa). I don't think their
are any hard numbers available for that since the number of uncontrollable
factors is so large.

Michael Hiteshew
Lockheed Martin NE&SS Marine Systems
410-682-1259



> ----------
> From:         Buscomb, Scott[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.;Buscomb, Scott
> Sent:         Monday, July 09, 2001 6:07 PM
> To:   [log in to unmask]
> Subject:      [TN] Pattern to Pattern Tolerance
>
> I am looking for the standard industry locational tolerance of copper
> feature to copper feature on a single sided PCB. Since PCB fabrication is
> a
> photographic process, I am assuming it is a function of gerber plotter and
> artwork imaging.
> TIA,
>
> Scott Buscomb
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2