TECHNET Archives

May 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bill Davis <[log in to unmask]>
Reply To:
"TechNet E-Mail Forum." <[log in to unmask]>, Bill Davis" <[log in to unmask]>
Date:
Mon, 24 May 1999 07:53:33 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (82 lines)
I agree with Werner- the only possible "goodness" that would come from
this is to run cycles at a high thermal gradient
(e.g., 20C/min or greater). Typical Blue M ovens that are 3X3X3 run at
7C/min maximum gradient. You would have to run at a thermal gradient so
steep that the board thermal mass becomes the limiting factor. Only then
would you find problems that are truly related to assembly and not, as
Werner has pointed out, make good product into bad product...

> Bill Davis, Ph.D.
> Diamond Multimedia Systems
> Senior Scientist
> Tel. 408.325.7868
> Cell. 408.888.5650
> e-mail: [log in to unmask]
>
>


-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Sunday, May 23, 1999 4:15 AM
To: [log in to unmask]
Subject: Re: [TN] reliability testing on compliant pin technology


Hi EG,
You did not say what you are trying to accomplish with an environmental
stress screening of -15 to 60 deg C. As ESS goes, this is not much of a
screen, and I am seriously wondering if you accomplish anything at all.
What
you do may serve as a Burn-In, but I can not imagine what latent defects
you
would screen out with -15 to 60 deg C cycling-compliant pins or not-
unless
you run it long enough to damage good product.

Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2