Kenny,

Refer to J-STD-001C section 9.2.4.3 "Partially Visible or Hidden Solder
Connections".  Basically says that such connections are acceptable as long
as the joints you CAN see are acceptable and process controls are
maintained.   ie: if the visible joints are good, the invisible ones must be
too!

In a former life we spent a lot of time and money x-raying solder fill of TH
soldered connectors with invisible joints.  This was because the customer
required the x-ray inspection.  We hardly ever saw cause for concern.  My
experience was that the most difficult to solder pins (in regards to being
tied to the most thermal plane within the PCB) are typically the power and
ground pins.  Conventional connector designs almost always have power and
ground pins as pin 1 or the last pin(s) of the connector row(s), and these
are almost always the outer (and visible) rows of the connectors.

Hope that helps,
Kevin Glidden



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, February 28, 2006 11:47 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Joint Inspection

Are they wave-soldered?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bloomquist, Ken
Sent: Tuesday, February 28, 2006 10:42 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Joint Inspection

Hi John,

Your assumption is correct, it is a through hole board. We have thermal
spokes around all internal layers but it still sucks up a lot of heat.

KennyB


-----Original Message-----
From: John Maxwell [mailto:[log in to unmask]]
Sent: Tuesday, February 28, 2006 8:20 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Joint Inspection
>
Ken,
I assume that these are thru hole solder joints. If they are then the only
inspection tool is x-ray. Was or could thermal relief be used around these
holes?

John

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2