Ken-

        A cheaper alternative to having MPM build their dedicated work holders is
to have your wave solder pallet shop build one.  I checked out the price of
both for our MPM printer and the pallet shop could make a "printer pallet"
for much, much less than the OEM.  Just something to think about.

Ryan Jennens
TelGen Corp.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jorge Engenharia
Sent: Tuesday, April 13, 1999 12:44 PM
To: [log in to unmask]
Subject: Re: [TN] Double sided reflow


Ken,
  Just to ad more info, the second side may need a special support on
screen printer in order to have acceptable board support, mainly if you
have fine pitch device on second side. This support is called "
dedicated workholder" by MPM guys, but you can built yourself using your
toolshop. Try MPM web site to see what a dedicated workholder looks
like.
  When we did double side reflow no problem were found using eutetic
solder paste.

Jorge Santana
Process Engr
Microtec - Brazil

> -----Original Message-----
> From: Stephen R. Gregory [SMTP:[log in to unmask]]
> Sent: 13 de Abril de 1999 12:20
> To:   [log in to unmask]
> Subject:      Re: [TN] Double sided reflow
>
> In a message dated 4/13/99 12:27:46 AM Pacific Daylight Time,
> [log in to unmask] writes:
>
> << Can someone help with the processing of a heavily populated SM PCB,
>  SM top and bottom which has to be reflowed both sides and has through
>  holes parts ( no wave solder ).
>
>  Any guidelines on how this should be processed would be of great
>  help ie what side is the high temp solder used on, most densly least
>  densly populated etc etc.
>
>  Regards,
>  ken Robertson
>  Telspec >>
>
> Hi Ken!
>
> I'm assuming that the reason you must do double sided reflow is
> because the
> board either has fine pitch or BGA's on both sides, am I correct? As
> far as
> using different melting point solders, I know there's some info out
> there
> that discusses that, but I really don't think that's a good thing to
> do. Just
> say for instance; what if somebody screws up and prints the wrong
> paste on
> the wrong side? You really don't need to do that anyway. Just about
> any
> component I can think of (as long as IPC guidlelines have been
> followed as
> far as pad layout and footprint) has enough surface tension to stay
> put when
> solder goes liquidous on the bottom...(provided your board isn't
> bowing and
> the reflow oven conveyer is smooth running).
>
> The exceptions to that are extremely heavy parts like ceramic or metal
> bodied
> QFP's and PLCC's, or parts with attached heatsinks. Sometimes Melfs
> will give
> you problems, or I've had problems with 4-leaded plastic body
> oscillators and
> certain filters too. Basically, suspect the parts that don't have much
> lead
> area to 'em. The figure I remember, and many people say this is pretty
> conservative, is that you'll have 30-grams of surface tension for
> every
> square inch of lead surface.
>
> As far as what side to do first, I usually leave the side that has the
> finest
> pitch on it for the last side. If ya got any other specific questions,
> let us
> know...
>
> -Steve Greory-
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2