TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dave Dixon <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Dave Dixon <[log in to unmask]>
Date:
Wed, 29 Oct 2008 16:17:08 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (62 lines)
Sounds funny.  The flux is "compliant", but they suggest that you use it
with tin/lead solder.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Wednesday, October 29, 2008 10:35 AM
To: [log in to unmask]
Subject: Re: Soldering to Aluminum?

Pete,

Seems to me there was recent thread here on something similar.  We have
soldered to stainless steel and I think the process is similar for
aluminum.  It has to do with the flux used.  Word of caution... I
believe it is an acid based flux so how it is applied and washed off may
be of concern.

From McMaster-Carr website:

Aluminum Soldering Flux

Use this paste flux with aluminum solder and any tin/lead solder to
solder aluminum and aluminum alloys. Also for use with copper, chrome,
and brass. Meets DOD 1866 and is ROHS compliant.
4-oz. Jar 7696A2   Each   $9.65
1-lb. Jar 7696A1   Each   $30.41

 I have not tried it.

Phil Nutting


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete Houwen
Sent: Wednesday, October 29, 2008 10:01 AM
To: [log in to unmask]
Subject: [TN] Soldering to Aluminum?

Has anyone tried soldering lead free to an Aluminum circuit on
polyester?

We are looking at a very simple one component circuit that needs to be
on a material with some flexibility.  We do run millions of feet of
aluminum on polyester passive circuits in one of our plants.  I am being
asked to see if we can take advantage of the in house production to save
some cost.

My other thought is to just try a conductive adhesive, but we might need
to do some tooling for that, as this would require about 3 million of
these circuits/year.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2