Doug,
We are currently using the eddy current method to measure our
conformal coating thickness. Recently we had some issues where one operator
was making adjustments to the coating thickness every time they measured the
thickness coupon. After a shift change the operators would run another
coupon through only to find that the coating was thicker then needed and
would change the settings back. What we found out was that the operators
were using varying amounts of pressure changing the readings on the meter
giving us measurements that were not in control. We now have an automated
system that applies the correct amount of pressure continually providing us
with more accurate readings.
Regards,
Ted T
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
Sent: Thursday, December 04, 2008 1:19 PM
To: [log in to unmask]
Subject: [TN] Conformal Coat and Eddy Currents
Good afternoon all,
A question for this most excellent forum. Does anyone here use eddy
current methods to measure applied coating thickness on printed circuit
assemblies? If so, can you share your opinions on the methods and the
equipment?
There are testers on the market that do this and one of our design
engineers is currently suprised at how we are using "stone age"
technologies (micrometer) to measure coating thickness.
Doug Pauls
Rockwell Collins
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|