Hi Prashant - the items of concern for the reballing operations would be:
1) temperature control of the deballing and reballing procedures; 2)
moisture levels/control of the BGA component; 3) cleanliness control of
the procedure in terms of ionic residues from the solder processes; 4) ESD
control; 5) physical damage control in terms of pad damage and soldermask
damage.
Dave Hillman
Rockwell Collins
[log in to unmask]
prashant chopra <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
11/11/2010 04:52 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
prashant chopra <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] BGA reballing -- ROHS to Lead solder balls
Hi,
We are having a ROHS BGA which we want to use in the Non-ROHS (leaded)
process. We are looking at option of having the BGA reballed. We would
have the ROHS solder balls removed and replaced with the Non-ROHS solder
balls.
I need help to know what can be the technical risks in using these BGA?
Also, what can be the risk and issues associated with this reballing
process?
Also, what are the critical precautions, checks and tests which should be
done after the reballing of the BGA before we use them on the PWB?
Thanks to all for the support and advice.
Rgds
prashant
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|