TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vUakc-0000ZbC; Mon, 2 Dec 96 09:57 CST
Encoding:
59 Text
Old-Return-Path:
Date:
Mon, 02 Dec 96 09:54:44 cst
Precedence:
list
Resent-From:
From [log in to unmask] Tue Dec 3 14:
46:14 1996
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/8110
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"okQ891.0.viK.unleo"@ipc>
Subject:
From:
"ddhillma" <[log in to unmask]>
X-Loop:
Cc:
Message-Id:
Parts/Attachments:
text/plain (69 lines)
     Hi David!
     
     I have done some initial investigating of the AlphaLevel finish and 
     was encouraged by its performance. The investigation results were 
     reported as part of the paper: "Wirebondability and Solderability of 
     Various Metallic Finishes for Use In Printed Circuit Assembly", SMI 
     Conference Proceedings, 1996, page 687.  A paper on the finish was 
     also published in the IPC 1996 Expo proceedings, "Alternative Metal 
     Finishes for Wire Bond and Soldering Applications", by Steve Beigle, 
     page S9-2. I think that there is quite a bit of room for more 
     investigation to be completed - there a several companies/individuals 
     working on testing right now. I believe that there will be a paper on 
     the finish at the IPC 1997 Expo too. Give Frank Kurisu, SolderMask Inc 
     of Huntington Beach CA 714-842-1987, a call for more info - they were 
     going to set up a plating tank and begin processing real product. I 
     have concerns on the possible migration of the finish under certain 
     conditions and voltages but the published SIR data to date has been 
     good. Good Luck.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]
     


______________________________ Reply Separator _________________________________
Subject: Anyone using AlphaLevel?
Author:  [log in to unmask] at ccmgw1
Date:    12/2/96 9:13 AM


Hi all,
     
Is anyone out there using AlphaLevel as a board finish?
     
If so, what are your thoughts:-
     
 Good?
 Bad?
 Ugly?
 Cheap?
 Expensive?
     
Any comments are appreciated.
     
  ________________________________________________________________________
 | [log in to unmask]         David Tandy. EDA Specialist.   GenRad ADS. | 
 | Tel: (+44) 161 491 9191     Orion Business Park, Bird Hall Lane,       | 
 | Fax: (+44) 161 491 9106     Stockport, Cheshire, SK3 0XG, England.     | 
 |________________________________________________________________________|
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2