TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
John Burke <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Date:
Mon, 1 May 2006 14:39:24 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (155 lines)
Very good points well made, thanks to both. As a collective between the
lead free forum and this group we have 3 major articles in the press in
the last two working days. The one in World Magazine,on Friday:

http://www.worldmag.com/articles/11798

The one I just put in Green Supply line Magazine (Thanks Gina) which
highlights how to get an exemption from lead free solder on
environmental grounds-:

http://www.greensupplyline.com/187002293

And the one published by Gordon in PCB 007

http://tinyurl.com/kmyuy

Anyone has contacts in Radio or TV let me know...............8-)

Anyone who is wondering why I have not been answering mail - this thing
had me up 'till one this morning and on the day job we are in the middle
of a package design................8-)

John


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dale Ritzen
Sent: Monday, May 01, 2006 2:01 PM
To: [log in to unmask]
Subject: Re: [TN] NTC Get the Lead Out

Werner,
Thank you very much for making my point better than I did... You are
going
to have to overcome years of this kind of misinformation and junk
science to
get to the common man who votes on a regular basis. The way to turn this
tide is to get them "informed", through any means possible that doesn't
make
you sound like you're trying to buck common "tribal knowledge". You have
to
hit them in the places they know best - like television and radio news
that
doesn't pander to one ideology or the other, so you get a fair rendering
of
your argument. The only non-aligned TV or radio network that comes to
mind
is the public radio and TV stations here in the States. However, they do
tend to be on the "green" side of things so logical arguments presented
via
that media may even come under attack from those that offer to present
the
facts.

I'm not saying that this can't be turned back through massive requests
for
exemption by every industry. In fact, that's a pretty good ploy until
your
stockholders get the word that you're "not green". 

Has anyone attempted to point either National Public Radio or affiliated
TV
stations toward John's Push Back website? If you're going to attack this
thing and kill it, we need to take a multi-pronged stab at it.

My 0.02 Euros worth... And I'll get off my soap box now...
Dale Ritzen
Quality Manager
Austin Manufacturing Services

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier
Sent: Monday, May 01, 2006 3:37 PM
To: [log in to unmask]
Subject: Re: [TN] NTC Get the Lead Out


Hi Dale,
Unfortunately you are citing another example of junk science pobular 
knowledge. 
"...they only know that drinking water from lead pipes (or with leaded 
solders) is bad for you."
The first part refers to the Roman aqueducts that contained lead linings
and

pipes-a study I read not too long ago actually attributes the
Pb-poisioning
of 
the roman nobility to the fact that they drank their wine [acitic] from 
Pb-leaching vessels [Brian, please correct me if I am wrong on this].
the
second 
one with the Pb-bearing solder used to solder copper water pipes is
definitely a 
red herring. 
In New Jersey, the copper pipes were initially replaced with PCP
pipes-these

leach indefinitely, but what was worse, they sand blasted the
Pb-containing 
paint off of highway bridges [how many kids have you seen chewing paint
off
of a 
highway bridge?] which of course made it air-borne and thus contaminated
the

backyards of people's houses close by.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2