Doug -
Tg of resin does not necessarily mean better thermal performance at
temperatures above the Tg - Tg is an indication of the degree of cure
for that resin system based on an expected value. Lead-free soldering
excursions are well in excess of Tg and what condition is most important
is the decomposition temperature of the base material. We have seen
that some lower Tg materials actually have a higher decomp temperature
than higher Tg materials. This should be studied with your board house
to find the correct material that meets your specific temperature
cycling for lead-free. There are also base materials that are
specifically designed to have high decomp temperatures and maintain
adequate electrical performance also. The trade off with these
materials is cost - both in base materials and in processing.
Jeff
Jeffrey Bush
Director, Quality Assurance and Technical Support
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302-1890
Tel. 802.257.4571.21 Fax. 802.257.0011
[log in to unmask]
http://www.vtcircuits.com
-----Original Message-----
From: McCall,Doug [mailto:[log in to unmask]]
Sent: Wednesday, May 19, 2004 3:02 AM
To: [log in to unmask]
Subject: [TN] Pb-free and laminate Tg requirements
Hi,
What is the general thinking on the glas transistion temp (Tg) for FR4
being used for Pb-free PCBAs. I guess that the 'standard' is 140 deg-C
and is it sensible (and required) to go for a higher Tg?? Is it a good
idea to use a higher spec laminate??
Any thoughts will be very interesting.
Thanks,
> Douglas I McCall
> Printed Circuit Board Assembly Engineer,
>
> /// /// /// BOC EDWARDS
H BOC Edwards, 15 Marshall Road, Eastbourne, East Sussex, England,
BN22
9BA
> * +44 (0)1323 501147
* +44(0)1323 509824
*+44 (0)7785 247 685
> * mailto:[log in to unmask]
www.bocedwards.com
***********************************************************************
This email is confidential and intended solely for the use of the
individual to whom it is addressed. Any views or opinions presented are
solely those of the author and do not necessarily represent those of the
BOC Group plc or any of its affiliates. If you are not the intended
recipient, be advised that you have received this email in error and
that any use, dissemination, forwarding, printing, or copying of this
email is strictly prohibited. If you have received this email in error
please return the message to the sender by replying to it and then
delete the message from your computer.
This footnote also confirms that this email message has been checked by
anti-virus software for the presence of computer viruses. However, the
BOC Group plc or any of its affiliates accepts no responsibility for any
virus or defect that might arise from opening this e-mail or
attachments.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|