TECHNET Archives

June 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Bob Carhart <[log in to unmask]>
Date:
Wed, 17 Jun 1998 12:02:30 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Karl Sweitzer <[log in to unmask]>
Subject:
From:
Karl Sweitzer <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Organization:
Image Acquisition Systems http://www.kodak.com/cgsHome/ias.shtml
Content-Type:
text/plain; charset=us-ascii
Parts/Attachments:
text/plain (44 lines)
Bob,

We recently went through this exercise.  Three that we found with
"low" outgassing (i.e. TML ~<1%) are:

EPIC 200
Morton Electronic Materials
Tustin, CA
714-730-4535
Contact: Lincoln Eramo

TAIYO PSR-4000BM
TAIYO America, Inc.
Carson City, NV
702-885-9959

CARAPACE EMP110 (with UV Bump)
Electra Polymers & Chemicals America
Orange, CA
714-744-8394
Contact: Lee Collier

All of these vendors supplied outgassing data.  You will have to run
these by your NASA materials person to final approval.

Good luck!
--
Karl Sweitzer                     voice: 716.47.77546
Eastman Kodak Company             pager: 716.25.33681
800 Lee Road                        fax: 716.47.77293
Rochester, NY 14650-3118         mailto:[log in to unmask]

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2