Bob, We recently went through this exercise. Three that we found with "low" outgassing (i.e. TML ~<1%) are: EPIC 200 Morton Electronic Materials Tustin, CA 714-730-4535 Contact: Lincoln Eramo TAIYO PSR-4000BM TAIYO America, Inc. Carson City, NV 702-885-9959 CARAPACE EMP110 (with UV Bump) Electra Polymers & Chemicals America Orange, CA 714-744-8394 Contact: Lee Collier All of these vendors supplied outgassing data. You will have to run these by your NASA materials person to final approval. Good luck! -- Karl Sweitzer voice: 716.47.77546 Eastman Kodak Company pager: 716.25.33681 800 Lee Road fax: 716.47.77293 Rochester, NY 14650-3118 mailto:[log in to unmask] ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################