Hi Brian,
I would appreciate pictures, possibly also to Steve, that I could use in my reliability column—this is a failure mode fairly new and unknown to most people.
If you could, I also would appreciate the base material, the peak reflow temperature, the cooling rate after reflow, the Cu trace thickness and whether it was covered with solder, and what solder. I now, its asking a lot, but only with all the pertinent info can we make sense of this.
Werner
-----Original Message-----
From: Brian Chandler <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, Feb 3, 2010 7:28 am
Subject: Re: [TN] track lifting
We just conducted a study on acceptable strain levels for lead free products.
Our BGA test coupons showed this exact result from excess strain.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|