Wade,
Martha from AMP has some good suggestions, but does not suggest
the best possible alternative. Check with TEKA Interconnect Systems
(www.tekais.com) and see if they have a solder bearing connector in the
style you require. The leadframes are already pre-loaded with solder and
flux, eliminating the paste requirement and the possibility of
bridging/shorting when inserting the connector onto wet paste. Just
slide 'em on and pop in the oven, they work great....
Mike McMonagle
PCA Process Engineering Supervisor
K*Tec Electronics
1111 Gillingham Lane
Sugar Land, TX 77478
(281) 243-5639 Phone
(281) 243-5539 Fax
[log in to unmask]
> -----Original Message-----
> From: Wade Oberle [SMTP:[log in to unmask]]
> Sent: Wednesday, April 07, 1999 3:18 PM
> To: [log in to unmask]
> Subject: [TN] soldering Connector
>
> Dear Technetters,
> I have a double side surface mount board with an edge
> connector.
> The connector slides on the edge and has leads on both sides on the
> board at a pitch of 0.05". There are about 30 leads on each side of
> the
> board. We are planning to attach this as one of the final assembly
> processes but how. Can we use a mini wave solder pot to create the
> solder joints or should we order a custom solder tip (0.05" x 1.68")
> so
> we can heat up all the leads on one side at one time and then feed in
> wire solder as needed?
>
> Any and all ideas would be appreciated. If anyone knows of an
> automated
> or semi-automated 'hot bar' solder method, we are interested.
>
> Thanks in advance for your assistance.
>
> Wade Oberle
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|