TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"McMonagle, Michael R." <[log in to unmask]>
Date:
Thu, 8 Apr 1999 08:44:20 -0500
MIME-Version:
1.0
X-To:
Wade Oberle <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "McMonagle, Michael R." <[log in to unmask]>
Parts/Attachments:
text/plain (73 lines)
Wade,
        Martha from AMP has some good suggestions, but does not suggest
the best possible alternative. Check with TEKA Interconnect Systems
(www.tekais.com) and see if they have a solder bearing connector in the
style you require. The leadframes are already pre-loaded with solder and
flux, eliminating the paste requirement and the possibility of
bridging/shorting when inserting the connector onto wet paste. Just
slide 'em on and pop in the oven, they work great....

Mike McMonagle
PCA Process Engineering Supervisor
K*Tec Electronics
1111 Gillingham Lane
Sugar Land, TX  77478
(281) 243-5639 Phone
(281) 243-5539 Fax
[log in to unmask]

> -----Original Message-----
> From: Wade Oberle [SMTP:[log in to unmask]]
> Sent: Wednesday, April 07, 1999 3:18 PM
> To:   [log in to unmask]
> Subject:      [TN] soldering Connector
>
> Dear Technetters,
>         I have a double side surface mount board with an edge
> connector.
> The connector slides on the edge and has leads on both sides on the
> board at a pitch of 0.05".  There are about 30 leads on each side of
> the
> board.  We are planning to attach this as one of the final assembly
> processes but how.  Can we use a mini wave solder pot to create the
> solder joints or should we order a custom solder tip (0.05" x 1.68")
> so
> we can heat up all the leads on one side at one time and then feed in
> wire solder as needed?
>
> Any and all ideas would be appreciated.  If anyone knows of an
> automated
> or semi-automated 'hot bar' solder method, we are interested.
>
> Thanks in advance for your assistance.
>
> Wade Oberle
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2