TECHNET Archives

May 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Tom Buschor <[log in to unmask]>
Date:
Wed, 22 May 2002 12:00:36 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Tom Buschor <[log in to unmask]>
Parts/Attachments:
text/plain (30 lines)
Linda,

Our data shows that using conformal coating as underfill can improve low
and high cycle fatigue life of BGA solder joints.

Years ago we conducted a test to compare the reliability of non-underfilled
BGAs, BGAs underfilled with a conformal coating material and BGAs
underfilled with reworkable epoxy. In general, BGAs underfilled with
conformal coating lasted longer than non-underfilled parts but failed
sooner than epoxy underfilled BGAs.

It depends on what type of BGAs are being underfilled and what conformal
coating material is being used as well as the test conditions.

I cannot share more without legal papers. If you wish to know more, contact
me offline.

Tom

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2