TECHNET Archives

January 2014

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Leland Woodall <[log in to unmask]>
Date:
Thu, 23 Jan 2014 19:07:54 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Message-ID:
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
In a previous life I did it, but not to find which one was best in class for solvent, but for which one was best in class for FIBERS. The reason was because the cheap stuff leaves lots of fibers inside the apertures of the stencils, in the paste, and on the surface of the stencil, and these showed up in the solder joints as well. We went to a different brand, it completely fixed the issue. I have not seen any issues with wipe solvent.
As part of this, I did notice a huge difference in overall quality of wipe paper between different vendors. I think we looked at 4 different vendors, but I do not remember which one we ended up using.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Thursday, January 23, 2014 12:36 PM
To: [log in to unmask]
Subject: [TN] Stencil Underwipe Solvents, Paper

Techsperts,

Has anyone out there conducted any experimentation with stencil underwipe solvents in an attempt to identify a best in class formulation?  In doing so, was it found that if a high quality paper is utilized the solvents actually did more harm than good?

Someone here has read something after a Google search, and questions are beginning to arise that I can't answer totally off the cuff.

Your help would be greatly appreciated, and offline replies are fine if you don't want to mention specific products or companies.

Thanks,

Leland



________________________________

“Confidentiality Notice:
This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments.”

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2