In a previous life I did it, but not to find which one was best in class for solvent, but for which one was best in class for FIBERS. The reason was because the cheap stuff leaves lots of fibers inside the apertures of the stencils, in the paste, and on the surface of the stencil, and these showed up in the solder joints as well. We went to a different brand, it completely fixed the issue. I have not seen any issues with wipe solvent. As part of this, I did notice a huge difference in overall quality of wipe paper between different vendors. I think we looked at 4 different vendors, but I do not remember which one we ended up using. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall Sent: Thursday, January 23, 2014 12:36 PM To: [log in to unmask] Subject: [TN] Stencil Underwipe Solvents, Paper Techsperts, Has anyone out there conducted any experimentation with stencil underwipe solvents in an attempt to identify a best in class formulation? In doing so, was it found that if a high quality paper is utilized the solvents actually did more harm than good? Someone here has read something after a Google search, and questions are beginning to arise that I can't answer totally off the cuff. Your help would be greatly appreciated, and offline replies are fine if you don't want to mention specific products or companies. Thanks, Leland ________________________________ “Confidentiality Notice: This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments.” ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________