Francis,
With regards to your question 1: There are pulse plating cycles reported in
the SURFIN98 that claim improved physical properties and thickness
distributions in the PTH. Would you be interested?
Richard Haynes
-----Original Message-----
From: Francis Lai <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Saturday, October 31, 1998 10:31 AM
Subject: [TN] Copper plating & Copper thickness
>Dear Sir :
>
>I work inn a high frequency PCB manufacturing company and I have the
>
>following questionns :
>
>1/ Why is it for copper plating (acid copper plating) the lower the
> current, the more the throwing power ? If I start to plate copper
> on the PTH walls with high current density after PTH, what will
> happen ?
>
>2/ Our customer always specify to have a certainn thickness innside the
> PTH walls for copper. Why is that so for high frequency PCB ?
> What happen if copper thickness is thinner than the specified
> thickness at high frequencies ?
>
>Thanks for your help !!!!!!!
>
>my e-mail : [log in to unmask](this is only text base, pls do not
send
> graphics)
>
>Thamks again!!!!!!!
>
>Francis
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|