TECHNET Archives

November 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 4 Nov 1998 16:37:31 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Richard Haynes <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Richard Haynes <[log in to unmask]>
Parts/Attachments:
text/plain (67 lines)
Francis,
With regards to your question 1: There are pulse plating cycles reported in
the SURFIN98 that claim improved physical properties and thickness
distributions in the PTH. Would you be interested?
Richard Haynes

-----Original Message-----
From: Francis Lai <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Saturday, October 31, 1998 10:31 AM
Subject: [TN] Copper plating & Copper thickness


>Dear Sir :
>
>I work inn a high frequency PCB manufacturing company and I have the
>
>following questionns :
>
>1/ Why is it for copper plating (acid copper plating) the lower the
>   current, the more the throwing power ? If I start to plate copper
>   on the PTH walls with high current density after PTH, what will
>   happen ?
>
>2/ Our customer always specify to have a certainn thickness innside the
>   PTH walls for copper. Why is that so for high frequency PCB ?
>   What happen if copper thickness is thinner than the specified
>   thickness at high frequencies ?
>
>Thanks for your help !!!!!!!
>
>my e-mail : [log in to unmask](this is only text base, pls do not
send
>                                      graphics)
>
>Thamks again!!!!!!!
>
>Francis
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2