Hi Tom;
Assuming this is the legend ink, Taiyo PSR-4000 is used for ENIG finish here. The Enig goes on first, then the legend, else discoloration occurs.
Is the finish gold?
Larry Russell
Consultant
Chant World Int'l
[log in to unmask]
http://www.chantworld.com
Tel No.: +886 3 452 5279
Fax No.: +886 3 452 0988
-----Original Message-----
From: Tom Burek [mailto:[log in to unmask]]
Sent: Friday, May 28, 2004 7:02 AM
To: [log in to unmask]
Subject: [TN] Purple Solder Mask
Greetings Technetters,
I have a circuit board that specifies Taiyo PSR-4000 white.
Some of the boards have a distinct purple tint to them.
Has anyone seen this phenomenon before?
Do you have any ideas what could cause it?
Thank you in advance.
Tom Burek, CID+
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|