TECHNET Archives

October 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 2 Oct 2013 06:34:08 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Geert Willems <[log in to unmask]>
Subject:
MIME-Version:
1.0
Message-ID:
Content-Type:
text/plain; charset="UTF-8"
Content-Transfer-Encoding:
quoted-printable
From:
Geert Willems <[log in to unmask]>
Parts/Attachments:
text/plain (8 lines)
A too strong blow-off of of the solder to get a flat finish by (one of) the HASL air knives will lead to insufficient solder coverage of the pads leading to unsolderable oxidized intermetallics after relatively short storage times. Since there is an airknive for each side, you may have an issue on only one side of the PCB which is rather unlikely for chemically deposited finishes like ImSn.