TECHNET Archives

October 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 2 Oct 2013 08:20:11 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Gerry Gagnon <[log in to unmask]>
Message-ID:
Subject:
From:
Gerry Gagnon <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (156 lines)
Hi Steve!
 
I would recommend you select a bare board from the stock that produced the assembly photos and take a picture of both sides. When taking the picture, if the pads exhibit a topography, try to take the pic at an angle that shows the topography. If the pads do not show a topography make sure the pics you select show that too.
 
With these pictures, I think we can all nail this one from the bare board side because the assembly pics tend to add some confusion.
 
Brs,
 
Gerry Gagnon

 
> Date: Tue, 1 Oct 2013 17:14:03 -0600
> From: [log in to unmask]
> Subject: Re: [TN] HASL question
> To: [log in to unmask]
> 
> Okay here's another picture. I printed a solder sample and sent it
> through the oven and this is what it looked like:
> 
> http://stevezeva.homestead.com/SolderSample.jpg
> 
> You can see all the non-wetting going on. The board  was profiled and it
> was fine. We are using a FCT Assembly WS889 SN100C solder paste.
> 
> What is even more strange is that the first side of the board looked
> okay, but the second side looks like in the photos, like the problem is
> confined to one side of the board if that's possible.
> 
> The solder sample was only reflowed once, but I printed the paste on the
> side that was to be built last. Weird huh?
> 
> I know you can't tell anything for sure just from some photos, but it's
> the strangest thing I've seen in a while... 
> 
> Steve 
> 
> -----Original Message-----
> From: Steve Gregory 
> Sent: Tuesday, October 1, 2013 4:46 PM
> To: [log in to unmask]; Steve Gregory
> Subject: RE: [TN] HASL question
> 
> Here's one picture:
> 
> http://stevezeva.homestead.com/NonWetting.jpg
> 
> Look at the left pad and the tarnish that you see there, does that look
> like tarnished nickel?
> 
> This is after the board was washed. I have places all over the board
> that looks like this. 
> 
> I'll post a picture of what it looks like after I printed a solder
> sample with paste and sent it through the reflow over
> 
> Steve 
> 
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
> Sent: Tuesday, October 1, 2013 4:16 PM
> To: [log in to unmask]
> Subject: Re: [TN] HASL question
> 
> Ahhhh....it's what I figured. I think that's what happened. I'll have
> pictures later.
> 
> Steve 
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
> Sent: Tuesday, October 1, 2013 4:15 PM
> To: [log in to unmask]
> Subject: Re: [TN] HASL question
> 
> No.  Not unless somebody screwed up.
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
> Sent: Tuesday, October 01, 2013 6:11 PM
> To: [log in to unmask]
> Subject: Re: [TN] HASL question
> 
> Hi all,
> 
> It's funny that the HASL topic has come up today, because we just ran a
> board today that supposedly was lead-free HASL finished, and man it
> looks like crap!
> 
> Question; does a PCB get nickel before it gets Lead-free HASL'ed?
> 
> Steve 
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev.
> PhD
> Sent: Tuesday, October 1, 2013 2:23 PM
> To: [log in to unmask]
> Subject: Re: [TN] HASL question
> 
> Hello Victor,
> 
>  It wouldn't solder in a first palce. 
> 
> --
> Best regards,
> 
> Vladimir Igoshev. PhD
> mailto:[log in to unmask]
> 
> SENTEC Testing Laboratory Inc.
> 11 Canadian Road, Unit 7.
> Scarborough, ON M1R 5G1
> Tel: (416) 899-1882
> Fax: (905) 882-8812
> www.sentec.ca
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
> service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
> service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
> service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
> service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
> 
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask] 
> ______________________________________________________________________
 		 	   		  

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2